1
很多新房的设计外面是砖或石的贴墙,很漂亮。但是这种会不会很难维护,因为接缝会
漏水?难道如果想省心,就只有土土的siding一种选择了么?
avatar
z*9
2
who told you '接缝会漏水?'
never heard of that.
avatar
w*r
3
墙里面有防水的。谁告诉你接缝漏水?用版砖拍他

【在 D*r 的大作中提到】
: 很多新房的设计外面是砖或石的贴墙,很漂亮。但是这种会不会很难维护,因为接缝会
: 漏水?难道如果想省心,就只有土土的siding一种选择了么?

avatar
B*4
4
真木头的siding最难维护老要刷漆。砖石的不用维护,但10-20年就要换,因为抹缝的
灰浆到时间就酥脆了,漏水。塑料或者金属siding不用维护,而且50年一换。
avatar
z*9
5
over 80% of houses in my neighborhood are brick or stone veneer, all of them
are more than 10 or 20 years old. never see anyone replace their brick or
stone veneer.

【在 B********4 的大作中提到】
: 真木头的siding最难维护老要刷漆。砖石的不用维护,但10-20年就要换,因为抹缝的
: 灰浆到时间就酥脆了,漏水。塑料或者金属siding不用维护,而且50年一换。

avatar
B*4
6
除非你在那住了20年,你怎么知道他们没换外墙?换的其实是木板上的防水层,砖可以
再用。买少量新砖就可以。

them
or

【在 z***9 的大作中提到】
: over 80% of houses in my neighborhood are brick or stone veneer, all of them
: are more than 10 or 20 years old. never see anyone replace their brick or
: stone veneer.

avatar
z*9
7
ok, I will ask someone to confirm that. I never heard of that. this
maintenance seems to be too huge to be true.

【在 B********4 的大作中提到】
: 除非你在那住了20年,你怎么知道他们没换外墙?换的其实是木板上的防水层,砖可以
: 再用。买少量新砖就可以。
:
: them
: or

avatar
B*4
8
不是你想象的那么难:
Repointing process
Sound mortar normally does not need to be removed from a building during the
repointing process, although such a practice is common. New mortar can be
designed to match the color and texture of existing mortar to avoid visual
aberrations. The repointing process begins by removing damaged pointing to a
depth equal to or slightly more than the width of the joint, or to the
point where sound mortar is reached. Depths greater than 2-1/2" or 4 cm
would be filled in several passes, allowing the mortar to cure for at least
24 hours. The joint profile would be as rectangular as possible as the new
pointing mortar should be allowed ample opportunity to bond with the masonry
unit.
Removal of old mortar between joints is done carefully to avoid damage to
masonry units. On very old buildings with soft materials, such as under-
fired brick, removal by hand is often the most effective to avoid damage.
Hard Portland cement mortar is usually removed with a grinder or power
circular masonry blade, taking care not to damage the masonry units.
Vertical joints in most cases are always done by hand or with small power
chisels.
Poor repointing work often raises the level of the mortar joint above the
face of the masonry unit, which causes the mortar edge to feather. Such a
process is aesthetically undesirable and can cause performance problems as a
thin layer of mortar will quickly erode. In addition, depending on the
nature of the mortar, mortar that rises above the level of the face of the
masonry unit can participate in damaging the arris or corner of the masonry
unit. In these cases, deteriorated mortar is often not removed to a
sufficient depth.

【在 z***9 的大作中提到】
: ok, I will ask someone to confirm that. I never heard of that. this
: maintenance seems to be too huge to be true.

avatar
z*9
9
good to know. thanks for the info.

the
a
least

【在 B********4 的大作中提到】
: 不是你想象的那么难:
: Repointing process
: Sound mortar normally does not need to be removed from a building during the
: repointing process, although such a practice is common. New mortar can be
: designed to match the color and texture of existing mortar to avoid visual
: aberrations. The repointing process begins by removing damaged pointing to a
: depth equal to or slightly more than the width of the joint, or to the
: point where sound mortar is reached. Depths greater than 2-1/2" or 4 cm
: would be filled in several passes, allowing the mortar to cure for at least
: 24 hours. The joint profile would be as rectangular as possible as the new

avatar
D*r
10
我上次去看一个自己卖的房子,四面砖墙,老头告诉我自从他建那个房子到
现在快40年,砖墙什么维护都没有做过。可是看上去情况很好。
老头没必要在这上面撒谎吧。

【在 B********4 的大作中提到】
: 除非你在那住了20年,你怎么知道他们没换外墙?换的其实是木板上的防水层,砖可以
: 再用。买少量新砖就可以。
:
: them
: or

avatar
l*u
11
如果是整砖的话,外墙就基本不用维护了。新的砖皮外墙,时间长了会有砖封变形,裂
缝,要修补一下,也不必全重新做。

【在 D******r 的大作中提到】
: 我上次去看一个自己卖的房子,四面砖墙,老头告诉我自从他建那个房子到
: 现在快40年,砖墙什么维护都没有做过。可是看上去情况很好。
: 老头没必要在这上面撒谎吧。

avatar
D*r
12
修补就是拿水泥重新糊糊就行吗?

【在 l*********u 的大作中提到】
: 如果是整砖的话,外墙就基本不用维护了。新的砖皮外墙,时间长了会有砖封变形,裂
: 缝,要修补一下,也不必全重新做。

avatar
D*r
13
光靠墙里的防水不够吧?否则要siding做什么呢?

【在 w********r 的大作中提到】
: 墙里面有防水的。谁告诉你接缝漏水?用版砖拍他
avatar
B*4
14
如果是维护良好的 brick siding,只需从新勾缝就可以了。砖的寿命,理论上是100年
,但是砌砖的砂浆,寿命短的多。检修墙面往往会发现局部渗漏的情况(观察外墙表面
就可看见),这个时候,需要局部拆砖,甚至需要把整面墙的砖拆了,修复里面的防水
层,木板层。